Test date | Expiry date | Result | Odometer reading |
2016-08-31 | 2017-09-21 | ✓ Pass | 130,212 |
- offside front lower Windscreen has damage to an area less than a 10mm circle within zone 'A' (8.3.1a)
|
2015-09-22 | 2016-09-21 | ✓ Pass | 127,842 |
2014-09-15 | 2015-09-20 | ✓ Pass | 111,697 |
- Windscreen has damage to an area less than a 40mm circle outside zone 'A' (8.3.1d)
- Offside Front Front constant velocity joint gaiter deteriorated, but preventing the ingress of dirt (2.5.C.1a)
- Under-trays fitted obscuring some underside components
|
2014-09-15 | - | ✗ Fail | 111,697 |
- Windscreen has damage to an area less than a 40mm circle outside zone 'A' (8.3.1d)
- Offside Front Front constant velocity joint gaiter deteriorated, but preventing the ingress of dirt (2.5.C.1a)
- Under-trays fitted obscuring some underside components
|
2013-09-21 | 2014-09-20 | ✓ Pass | 107,133 |
2012-09-15 | 2013-09-14 | ✓ Pass | 98,399 |
- Windscreen has damage to an area less than a 10mm circle within zone 'A' (8.3.1a)
- brake disc worn, pitted or scored, but not seriously weakened (3.5.1i)
- Tyre worn close to the legal limit (4.1.E.1)
- Front Brake pad(s) wearing thin (3.5.1g)
|