Test date | Expiry date | Result | Odometer reading |
2018-05-04 | 2019-05-04 | ✓ Pass | 140,195 |
- Offside Rear Inner brake disc worn, pitted or scored, but not seriously weakened face (3.5.1i)
- Nearside Rear Inner Brake pad(s) wearing thin (3.5.1g)
|
2017-04-12 | 2018-05-04 | ✓ Pass | 132,598 |
2016-05-05 | 2017-05-04 | ✓ Pass | 127,033 |
2016-05-05 | - | ✗ Fail | 127,033 |
2014-11-17 | 2015-11-16 | ✓ Pass | 114,795 |
2013-11-05 | 2014-11-09 | ✓ Pass | 107,259 |
- Front Brake pad(s) wearing thin (3.5.1g)
|
2012-11-09 | 2013-11-09 | ✓ Pass | 96,958 |
- Steering column damaged but serviceable (2.2.C.1d)
|
2012-11-09 | - | ✗ Fail | 96,958 |
- Offside Front Tyre worn close to the legal limit (4.1.E.1)
- Steering column damaged but serviceable (2.2.C.1d)
|
2011-10-27 | 2012-11-09 | ✓ Pass | 79,283 |
2010-10-22 | 2011-11-09 | ✓ Pass | 63,450 |
- Offside Front Front suspension has slight play in a lower suspension ball joint (2.5.B.1a)
|
2010-10-22 | - | ✗ Fail | 63,450 |
- Offside Front Front suspension has slight play in a lower suspension ball joint (2.5.B.1a)
|
2009-11-02 | 2010-11-09 | ✓ Pass | 47,926 |
- Nearside Front brake disc worn, pitted or scored, but not seriously weakened (3.5.1i)
- Offside Front brake disc worn, pitted or scored, but not seriously weakened (3.5.1i)
- Offside Rear Brake pad(s) wearing thin (3.5.1g)
- Rear number plate starting to delaminate
- O/S/R brake disc corroded
- slight corrosion starting to appear on the O/S/R coil spring
|
2009-11-02 | - | ✗ Fail | 47,926 |
- Nearside Front brake disc worn, pitted or scored, but not seriously weakened (3.5.1i)
- Offside Front brake disc worn, pitted or scored, but not seriously weakened (3.5.1i)
- Offside Rear Brake pad(s) wearing thin (3.5.1g)
- Rear number plate starting to delaminate
- O/S/R brake disc corroded
- slight corrosion starting to appear on the O/S/R coil spring
|