Test date | Expiry date | Result | Odometer reading |
2018-03-21 | 2019-03-31 | ✓ Pass | 127,782 |
- Offside outer sill corroding
- Nearside outer sill corroding
- corrosion on floor pans
- exhaust corroded
|
2018-03-21 | - | ✗ Fail | 127,782 |
- Offside outer sill corroding
- Nearside outer sill corroding
- corrosion on floor pans
- corrosion on front subframe
- Front corrosion on front suspension components
- Offside Front Tyre worn close to the legal limit (4.1.E.1)
- Offside Rear tyre wearing inner and outer edge and tyre feathering inner edge
- Nearside Front tyre wearing inner and outer edge
- exhaust corroded
- Offside Rear Registration plate lamp not working (1.1.C.1d)
- Exhaust emissions carbon monoxide content at idle excessive (7.3.D.4)
- Exhaust emissions carbon monoxide content after 2nd fast idle excessive (7.3.D.3)
- Exhaust emissions hydrocarbon content after 2nd fast idle excessive (7.3.D.3)
- Exhaust emissions Lambda reading after 2nd fast idle outside specified limits (7.3.D.3)
|
2017-03-27 | 2018-03-31 | ✓ Pass | 120,896 |
- exhaust corroded
- Offside Rear tyre stepped
|
2017-03-27 | - | ✗ Fail | 120,896 |
- exhaust corroded
- Offside Rear tyre stepped
- Front pads low
|
2016-03-21 | 2017-03-31 | ✓ Pass | 112,010 |
- corrosion on inner and outer sills
- exhaust heatshield loose above backbox
- Offside Front cv gator perishing
- Nearside Front cv gator perishing
- Offside Front tyre on legal limit
- Front roll bar bushes link bushes perishing
|
2016-03-21 | - | ✗ Fail | 112,008 |
- corrosion on inner and outer sills
- exhaust heatshield loose above backbox
- Offside Front cv gator perishing
- Nearside Front cv gator perishing
- Offside Front tyre on legal limit
- Front roll bar bushes link bushes perishing
|
2015-03-24 | 2016-03-31 | ✓ Pass | 104,385 |
- front link pin bushes perished
- cv boots badly cracked
|
2015-03-24 | - | ✗ Fail | 104,385 |
- e,m,l on dash
- front link pin bushes perished
- cv boots badly cracked
|
2014-03-12 | 2015-03-31 | ✓ Pass | 155,852 |
- o/s outer sill corroded
- inner sills showing signs off corrosion
|
2014-03-12 | - | ✗ Fail | 155,852 |
- engine management lamp on
- o/s outer sill corroded
- inner sills showing signs off corrosion
- n/s/f tyre tread low and cracking and splitting outer edge of tread
|
2013-03-18 | 2014-03-31 | ✓ Pass | 92,580 |
- stonechip in screen.
- oil leaks.
- slight wear to o/s/r shockabsorber lower bush.
- coil springs corroded.
- exhaust cat corroded.
- various suspension bushes perished and cracking.
- cv gaiters cracking.
|
2013-03-18 | - | ✗ Fail | 92,580 |
- stonechip in screen.
- oil leaks.
- slight wear to o/s/r shockabsorber lower bush.
- coil springs corroded.
- exhaust cat corroded.
- various suspension bushes perished and cracking.
- cv gaiters cracking.
|
2012-03-26 | 2013-03-31 | ✓ Pass | 90,178 |
- Offside Front Steering system has slight free play detected at steering wheel (2.2.A.1b)
- Nearside Front Front constant velocity joint gaiter deteriorated, but preventing the ingress of dirt (2.5.C.1a)
- Offside Front Front constant velocity joint gaiter deteriorated, but preventing the ingress of dirt (2.5.C.1a)
- Offside Front Anti-roll bar linkage rubber mounting deteriorated but not resulting in excessive movement (2.4.G.2)
- Rear Brake hose has slight corrosion to ferrules (3.6.B.4e)
- Nearside Rear Tyre worn close to the legal limit (4.1.E.1)
- underseal
|
2011-03-24 | 2012-03-31 | ✓ Pass | 88,385 |
- Windscreen has damage to an area less than a 10mm circle within zone 'A' (8.3.1a)
- Windscreen has damage to an area less than a 40mm circle outside zone 'A' (8.3.1d)
- Nearside Front Front constant velocity joint gaiter deteriorated (2.5.C.1a)
- Offside Front Front constant velocity joint gaiter deteriorated (2.5.C.1a)
|
2011-03-24 | - | ✗ Fail | 88,385 |
- Windscreen has damage to an area less than a 10mm circle within zone 'A' (8.3.1a)
- Windscreen has damage to an area less than a 40mm circle outside zone 'A' (8.3.1d)
- Nearside Front Front constant velocity joint gaiter deteriorated (2.5.C.1a)
- Offside Front Front constant velocity joint gaiter deteriorated (2.5.C.1a)
|
2010-03-09 | 2011-03-31 | ✓ Pass | 83,063 |
- exhaust front section corroded , corrosion to various body panels , cracking to outer c.v gaiters
- front anti roll bar drop link bushes worn
- wear to rear shock absorber lower bushes
- ribbed belt heavily cracked
|
2010-03-09 | - | ✗ Fail | 83,063 |
- exhaust front section corroded , corrosion to various body panels , cracking to outer c.v gaiters
- front anti roll bar drop link bushes worn
- wear to rear shock absorber lower bushes
- ribbed belt heavily cracked
- o/s/r tyre worn to limit
- slight cracking to n/s/f tyre
|
2009-03-22 | 2010-03-31 | ✓ Pass | 76,696 |
2009-03-22 | - | ✗ Fail | 76,696 |
- Ribbed belts cracking Stonechips in windscreen Fluctuation to front brake readings Front pads worn very low Front brake discs corroded & worn Coil springs corroded NSR tyre worn & perished Alloy wheels in poor condition
|
2008-03-22 | 2009-03-31 | ✓ Pass | 60,081 |
- front wipers split , front brake discs worn/lipped , damage to wheel rims
|
2008-03-22 | - | ✗ Fail | 60,081 |
- front wipers split , front brake discs worn/lipped , damage to wheel rims
|
2007-03-14 | 2008-03-31 | ✓ Pass | 42,342 |